Hi all
Just finished setting up my equipment and tried it out on a rusty no6 iron cap. didn't think it would be sooooooo good. Cap came out of the electrolytic bath like new. Was so in a hurry to see what it could do that I forgot to take photo's. Will post before and after for the next item and see what you guys think. Its amazingly simple and only uses washing soda, a stainless steel tub ( I used an old deep fat fryer pan ) and a battery charger. Photo's to follow.
Just finished setting up my equipment and tried it out on a rusty no6 iron cap. didn't think it would be sooooooo good. Cap came out of the electrolytic bath like new. Was so in a hurry to see what it could do that I forgot to take photo's. Will post before and after for the next item and see what you guys think. Its amazingly simple and only uses washing soda, a stainless steel tub ( I used an old deep fat fryer pan ) and a battery charger. Photo's to follow.