Not with good quality hot dipped Krome. BZP deffinitely. The wisdom I was always told by old non-yachty boatbuilders is that the galv acts to wear with the steel/iron. Certaily the good old Galv nails lasted better than copper on a heavy exposed roof....can only say what my relatively limited experience is.That's interesting and contrary to everything I've read... The usual spin on things is that the movement of the slates wheres off the galvanisation and creates a weak point on the nail, which corrodes and leads to slipped slates etc. But not in your experience?