Yojevol
Clocking on
10 slabs of Cherry timber photographed both sides:-
In general heartwood is in good condition, however there is worm damage in the sapwood although it's not active having been treated, I've marked were there is a bit of damage in the heartwood. The exception is F where there is evidence on one side but not the other so I've assumed its thickness is only 1".
Collection from GL19
Brian
Cherry | L | T | W | V | Price @ £35/cu.ft |
A | 81 | 2.5 | 8.63 | Sold | |
B | 78 | 2.5 | 9.71 | 1.10 | Sold |
C | 80 | 2.5 | 9.83 | 1.14 | 40 |
D | 81 | 2.5 | 9.42 | 1.10 | Sold |
E | 78 | 2.25 | 9.63 | 0.98 | Sold |
F | 77 | 1 | 7.42 | 0.33 | 12 |
G | 78 | 2.5 | 8.08 | 0.91 | 32 |
H | 80 | 3 | 6.25 | 0.87 | 30 |
I | 60 | 3 | 11.92 | 1.24 | Sold |
J | 59 | 2.5 | 11.25 | 0.96 | 34 |
In general heartwood is in good condition, however there is worm damage in the sapwood although it's not active having been treated, I've marked were there is a bit of damage in the heartwood. The exception is F where there is evidence on one side but not the other so I've assumed its thickness is only 1".
Collection from GL19
Brian